Epoxy Resin L and Hardener L 40 min. (240g) 200g Resina / 40g Hardener br>
The resin system Epoxy Resin L + Hardener L yields superior impregnating and wetting properties towards carbon, glass, aramid and natural fibres.

Low viscosity
Highly transparent
High degree of UV stability
Tack-free curing even of thin layers
Glass transition temperature (Tg) max. 76 °C (post-curing at 60 °C / 15 h)
High static and dynamic strength
Free of nonylphenol and DETA
Processing time: 40 minutes (100 g / 20 °C)
Mixing ratio:
100 : 40 parts by weight resin : hardener
100 : 45 parts by volume resin : hardener
It exhibits a very good price/performance ratio and is suitable for the following processing procedures:
Hand laminating
Vacuum moulding
Press moulding
Expertise for the resin system Epoxy Resin L + Hardener L: this system is not cytotoxic (cell damaging), important for applications in medical purposes.
Mechanical properties (Neat resin after curing)
Flexural test
Flexural strength (DIN EN ISO 178): 111 MPa
Flexural modulus (DIN EN ISO 178): 2.960 MPa
Tensile test
Tensile strength (DIN EN ISO 527): 69 MPa
Elongation at break: 4.7 %
Compression test
Compressive strength (DIN EN ISO 1426): 91 MPa
PoxySystems® is a registered trademark of R&G
General information about the system "Epoxy Resin L" with Hardeners S, L, CL, EPH 500, EPH 161, W 300, GL 1 and GL 2
* Low viscosity, free of solvents and fillers
* Fast impregnation of glass, aramid, carbon and natural fibres
* High static and dynamic strength (GL approval with the Hardeners GL 1 and GL 2 being present

Epoxy Resin L with the corresponding Hardeners S, L, CL, EPH 500, EPH 161, W 300, GL 1 and GL 2 is the most commonly used laminating and adhesive resin in R&G`s delivery programme.

In conjunction with the Hardeners S (15 minutes), L (40 minutes), CL (60 minutes), EPH 500 (60 minutes), EPH 161 (90 minutes), W 300 (300 minutes), GL 1 (30 minutes) and GL 2 (210 minutes), this epoxy resin exhibits similar mechanical properties to those of the laminating systems usual aerospace .Its heat deflection temperature reaches from 60 °C (S, L, EPH 500, W 300), to 80 °C (GL 1 and GL 2, after post-curing), to 95 °C (CL, after post-curing) and finally to 120 °C (EPH 161, after post-curing).

Its low surface tension, good adhesion, and minimal curing shrinkage makes the Epoxy Resin L ideal for bonding wood, metal, foamed polystyrene like Styropor® etc. It can be processed in all of the customary methods, e.g. hand lay-up, pressure and vacuum impregnation, press moulding and filament winding.



few units
few units

Reviews
We Accept
Quick Find
 
Use keywords to find the product you are looking for.
Advanced Search
Manufacturers
Manufacturer Info
R-G.de
R-G.de Homepage
Other products
Languages
Español English
Currencies